What a DFM review actually does

A good review reads the geometry the way the mold will see it. Where does the part release from the core? Where are the thick sections? Which surface will show every small defect? The answers shape the tool design and often the part design too.

The output should be a written list of concerns and suggestions, not a single approval. You want to know what to change and what happens if you do not.

Draft and radii

Plastic shrinks onto the core as it cools, so a vertical wall grips the steel and fights ejection. A small draft angle lets the part release cleanly. A common starting point is about one degree for every 25 mm of cavity depth, though the material changes that.

Rounded corners help resin flow and reduce stress concentration. They also make the mold easier to polish. Sharp internal corners are hard to machine and tend to crack over time.

Walls, ribs and bosses

Keep walls even. Where you need strength, use ribs rather than a thicker wall, and keep a rib near half the thickness of the wall it joins. Bosses need the same care; a solid boss is a thick section waiting to sink.

Coring out the inside of a boss removes material without losing the screw feature. It is one of the cheapest DFM wins on many parts.

Four DFM checks and what happens if you skip them
FeatureStarting pointIf you ignore it
DraftAbout 1° per 25 mm of depthThe part sticks in the core
RibAbout half the wall thicknessSink on the visible face
Inside radiusAdd a radius at cornersStress cracks and slow polishing
BossCore out the insideHeavy section and long cooling

Gates, vents and parting lines

Ask for the DFM in writing

A one-word approval is not a review. Ask for a list of concerns, the reason for each and what happens if you leave the design as it is. That list is the part of DFM you can act on before steel is cut.

Where the resin enters the cavity affects weld lines, flow marks and pressure. Put the gate where it fills evenly and where the mark will not be seen. Vents let trapped air escape; without them the part can burn or short shot.

The parting line leaves a faint mark. Plan where it falls, especially on a cosmetic face. It is easier to move on screen than on a finished tool.

When to do it

As early as possible. A change to wall thickness or draft costs almost nothing in CAD and can save weeks of rework on a tool. Once steel is cut, the same change becomes a modification.

If you are about to send an RFQ, include the drawing and ask for DFM feedback alongside the quote.