The short answer
Pick the steel from the job, not from a price list. For unfilled plastics and runs under roughly 300,000 shots, P20 is usually enough. Move to H13 when the resin is glass-filled or the run is long. Choose S136 when the part needs an optical finish or the resin is corrosive.
That is the whole rule in one paragraph. The rest of this guide explains where each line comes from, because the boundaries are not hard numbers and a supplier who quotes one grade for every job is not doing much engineering.
What the grade names mean
P20 is a pre-hardened steel supplied around 28–35 HRC. It arrives ready to machine, so there is no heat-treatment step waiting in the schedule. H13 is a hot-work tool steel, hardened after rough machining to about 44–52 HRC. S136 is a stainless mold steel, typically 48–55 HRC after treatment, with enough chromium to resist corrosion and enough cleanliness to take a mirror polish.
These are families, not single recipes. Different suppliers sell equivalents under their own names, so ask for the hardness range and the heat-treatment record rather than trusting a brand on a quote.
P20, H13 and S136 side by side
| Grade | P20 | H13 | S136 |
|---|---|---|---|
| As supplied | Pre-hardened, 28–35 HRC | Hardened after machining, 44–52 HRC | Hardened, 48–55 HRC, stainless |
| Typical volume, unfilled resin | Under 300k shots | 500k and above | 300k–1M+, finish dependent |
| Glass or mineral filled | Not recommended | Good default | Good where corrosion also matters |
| Corrosive resin (PVC, POM, FR) | Poor | Adequate with care | Best choice |
| Surface finish | Texture and satin | High gloss to A2 polish | Optical / A1 mirror |
| Relative tool cost | Baseline | Roughly +20–40% | Roughly +40–60% |
| Weld repair | Easiest | Possible with preheat | Most demanding |
Treat the cost column as a bracket, not a quote. Part size and cavity count can move the number more than the steel does on a small tool.
Resin decides first
Standard ABS, PP, PE and HIPS are gentle on steel. P20 handles them well at moderate volume and is the reason so many appliance and consumer molds are built from it. Our overview of mold types and capabilities shows where that grade normally appears.
Glass-filled nylon, mineral-filled PP and other reinforced resins are a different story. The fibres are abrasive. They erode gates and parting lines, and a P20 cavity can show measurable wear within the first 50,000 shots. H13 at the higher end of its hardness range is the usual answer. If the tool also has to survive a flame-retardant additive, S136 earns a second look.
Corrosion is the quiet failure mode. PVC, acetal and halogenated flame retardants can release by-products that pit an ordinary cavity over a long run. The mold does not break; the surface slowly roughens and parts start sticking or losing their finish. S136 is the practical fix, and it is far cheaper than re-polishing a cavity halfway through production.
Volume is the second filter
Below about 100,000 shots, P20 nearly always wins on total cost. Between 100,000 and 500,000, the answer depends on resin and finish. Above 500,000 shots, start the conversation at H13 unless there is a corrosion or optical reason to go straight to S136.
There is a useful calculation here. Take the price difference between the two grades and divide it by the extra shots the harder steel is expected to deliver. If the result is a few cents per shot, the upgrade is cheap insurance. Our guide to what drives injection mold cost uses the same cost-per-shot way of thinking.
One caution from our own work: production often grows after the tool is built. If your forecast sits within about 30% of a grade boundary, build in that buffer. A tool specified for 300,000 shots that ends up running 400,000 is a common reason for an unplanned rework visit.
Finish decides more than people expect
Texture, matte and satin finishes are available on all three grades. High gloss is where they separate. H13 can be polished to a good cosmetic standard, but S136 holds an A1 optical surface far longer, especially on clear PC or PMMA parts where any micro-pitting shows up immediately.
For medical and food-contact parts the reasoning is similar. Cleanability and surface stability matter over the life of the tool, not just at first sample. That is why our medical mold work tends to specify stainless forming surfaces even when the volume would not demand it.
You do not need one steel everywhere
A cost-effective mold often mixes grades. The base and support plates can be P20 while only the cavity and core inserts are H13 or S136. Only the surfaces touching the plastic need the wear or corrosion resistance, so this keeps the tool competitive without shortening its life.
The constraint is thermal expansion. P20 and H13 expand at similar rates, which makes interference fits stable across normal processing temperatures. Mixed insert stacks with very different alloys need a fit calculation from the toolmaker. It is worth asking about at design review, not after the first heating cycle.
Runner choice intersects with this decision too. A hot runner concentrates heat and wear at the gate, which is often the first place a tool needs attention. Our comparison of hot runner and cold runner molds covers that side of the design.
What to put in the RFQ
Ask for the steel grade and its equivalent standard, the hardness range after treatment, and who performs the heat treatment. On a high-value tool, ask whether material certificates are available. On expensive blocks, some buyers specify third-party material identification before machining begins; that check costs a few hundred dollars and occasionally catches a substituted grade.
Then ask for two quotes: the lowest-cost steel that meets the spec and the upgraded option. Seeing both numbers with the expected shot life beside them turns a technical question into a business decision. The RFQ checklist lists the other details engineers need to price a tool accurately.
Tell us your resin, annual volume and surface requirement. We will recommend a steel grade and explain why.
Send a drawing for a quote →Watch the process